Vinyl ink - Karlam
(Vinyl Base Reverse Printing Gravure Lamination Inks for PET Film)
Description: KARLAM Inks are formulated to offer sharp printability for solid and halftone jobs on Polyester Film, at quite a wider range of Press Speeds.
Application: KARLAM Inks offer good Adhesion on Polyester (untreated, unprimed and plain) film and are meant for Reverse Printing. These Inks are not suitable for Surface Printing Application.
Printing Process: Roto Gravure Printing only.
Printing Substrate: Polyester (untreated, unprimed and plain) film. Can be printed on Corona Treated BOPP Film, with 38 – 42 Dyne/Cm treatment level on the printing side, by adding a recommended dose of an Additive to these Inks.
Lamination: KARLAM Inks are suitable for Adhesive Lamination with Polyethylene Film, Aluminum Foil, Paper and Board. Lamination Peel Strength is depended on Adhesive used, its coating weight, Ink Coating weight, Substrates laminated, nature of jobs etc. It’s desirable to select right Adhesive applied with proper coating weight to get the best result.
Key Product Features:
- Good Bond Strength.
- Excellent printability resulting in clean and sharp images.
- Extremely stable and excellent re-usability.
- Excellent half tone reproduction.
- Colour Range: A full range of colours are available. Specific Shades are matched on Demand.
- It is desirable that User mentions his/her special requirements regarding Light Fastness, ARSR Properties or any other specific requirement of that sort beforehand while placing his/her indent with us.
- Desired shades can be obtained by intermixing standard colors at press room level.
Solvent System:
Normal | Toluene : Ethyl Acetate → 50 : 50 |
---|---|
Slowing the drying | Toluene : Ethyl Acetate : MIBK → 50 : 40 : 10 |
Accelerator | Ethyl Acetate or MEK |
Retarder | MIBK (as required, extra may lead to blocking) |
Shelf Life: The inks and medium of this series have, under normal conditions, a shelf life of at least 6 months
Normal Conditions means:
- Storage in tightly closed containers.
- No admixtures.
- Short time excessive-temperatures e.g. at transport are not harmful.
- The products are not sensitive to frost.
Over-stored inks (typical symptoms: fall in gloss, shift in shade, formation of odour and / or viscosity increase) may normally – (off color being exceptions) - be used the same way as residual inks by controlled admixture to fresh inks. Increased viscosity due to long-time storage of inks may generally be adjusted
by addition of a slightly higher amount of thinner than the usual.
Please take note of the following:
- The performance results indicated in this literature are only indicative under controlled conditions of laboratory with virgin & standard packaging grade films. Please do not use lower grades or substandard films. Karjen Industry will not take any responsibility for abnormal results
- Liability: While the information outlined is given in good faith, it does not constitute a guarantee and neither is one implied as to the specific end use suitability of any product. The customers should always evaluate the suitability of products to their own satisfaction
- Karjen Industry is responsible only to the tune of replacing the ink consumed in case of any printing related problems clearly assigned to in-compatibility
Health and Safety:
Read the health and safety guidelines before using these products. The user is responsible for all local Legislation requirement and packaging conditions.
Ink Handling: Please refer to general guideline for handling inks for flexible packaging. For further information, please contact Karjen Industry